Advanced Ceramic Igniters For Reliable Performance



A long-time expert in the field of ceramic igniters, CoorsTek provides reliable and long-life ceramic igniters in hot surface ignition (HSI) systems and ceramic spark igniters.

CoorsTek Electrosurgical Components

Model 101 Ceramic Igniter


120V Igniter – element made with UltraSiC® recrystallized silicon carbide. Reaches 1800 degrees Fahrenheit in 60 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 201 Ceramic Igniter


120V Igniter – element made with UltraSiC recrystallized silicon carbide. Reaches operating temperature in 34 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 271 Ceramic Igniter


120V Igniter – element made with UltraSiC recrystallized silicon carbide. Reaches operating temperature in 17 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 301 Ceramic Igniter


12 V Igniter – element made with proprietary ceramic composite. Reaches 1800 degrees Fahrenheit in < 3 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 401 Ceramic Igniter


24 V Igniter – element made with proprietary ceramic composite. Reaches 1800 degrees Fahrenheit in < 3 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 501 Ceramic Igniter


120 V Igniter – element made with UltraSiC recrystallizes silicon carbide. Reaches 2000 degrees Fahrenheit within 40 seconds @ 116 volts. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 601 Ceramic Igniter


120 V Igniter – element made with proprietary ceramic composite. Reaches 1800 degrees Fahrenheit in < 5 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 656 Ceramic Igniter


170-280 V Igniter – element made with proprietary ceramic composite. Reaches 1800 degrees Fahrenheit in < 3 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 726 Ceramic Igniter


220 V sheathed igniter – element made with proprietary ceramic composite. Reaches 1800 degrees Fahrenheit in < 7 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. . learn more arrows


CoorsTek Electrosurgical Components

Model 736 Ceramic Igniter


230 V sheathed igniter – element made with proprietary ceramic composite. Reaches 1800 degrees Fahrenheit in < 7 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


CoorsTek Electrosurgical Components

Model 746 Ceramic Igniter


240 V sheathed igniter – element made with proprietary ceramic composite. Reaches 1800 degrees Fahrenheit in < 7 seconds. Holder material available in standard and custom designs in steatite, cordierite, and alumina. learn more arrows


Ceramic Hot-Surface Igniters General Information


General overview of CoorsTek Igniter Product line inlduing 25-plus-year history and the division of traditional and mini igniters. Two-page PDF – 707 MB. download now arrows
 

DURAGLO Universal Silicon Nitride Igniter Replacement Kit


Click here for a listing of compatible models replaceable by the Duraglo Universal Silicon Nitride Igniter Replacement Kit.

 

Ceramic Hot-Surface Heating Igniters Brochure


Performance and dimension specifics for both traditional and mini igniter product lines. Two-page PDF – 757 MB. download now arrows



Ceramic Spark Igniters Brochure ENGLISH


General overview of ceramic spark igniters for stoves and heaters in English. Two-page PDF – 1.1 MB. download now arrows



Ceramic Spark Igniters Brochure PORTUGUESE


General overview of ceramic spark igniters for stoves and heaters in Portuguese. Two-page PDF – 1.3 MB. download now arrows