AD-85
Nominal 85% Al2O3

AD-90
Nominal 90% Al2O3

AD-94
Nominal 94% Al2O3

AD-96
Nominal 96% Al2O3

FG-995
Nominal 98.5% Fine-Grained Al2O3

AD-995
Nominal 99.5% Al2O3

AD-998
Nominal 99.8% Al2O3

PlasmaPure™ High-Purity Alumina
Minimum 99.8% Al2O3

PlasmaPure-UC™ Ultra-High-Purity Alumina
Minimum 99.9% Al2O3

YDA999E
Y2O3 Doped Al2O3