Food and Beverage

CoorsTek offers a variety of NSF-certified materials specifically designed for use in food processing and beverage handling equipment. These high-purity alumina ceramics provide excellent corrosion and wear resistance. Ideal for applications over a wide range of temperatures. Click here for a copy of our certification.

Contact Information:
Food and Beverage Handling Ceramics Specialists
+1.800.821.6110 Toll Free in North America
+1.303.277.4766 Tel
+1.303.277.4779 Fax

Related Literature:
Ceramic Material Properties Chart
PDF Document, Multi-Page, Printer Friendly (84 K)
Can Tooling and Handling Ceramics
PDF Document (177 KB)
Fluid Handling Ceramic Components
PDF Document (218 K)
Labware Catalog
PDF Document (342 K)
Labware Price List
PDF Document (157 K)


      AD-85 AD-90 AD-94 AD-96 FG-995 AD-995
Properties*   Units Test Nom. 85% Al2O3 Nom. 90% Al203 Nom. 94% Al203 Nom. 96% Al203 Nom. 98.5% Al203 Nom. 99.5% Al203
Density   gm/cc ASTM-C20 3.42 3.60 3.70 3.72 3.80 3.90
Crystal Size Average MICRONS THIN-SECTION 6 4 12 6 6 6
Water Absorption   % ASTM-373 0 0 0 0 0 0
Gas Permeability   0 0 0 0 0 0
Color   WHITE WHITE WHITE WHITE WHITE IVORY
Flexural Strength (MOR)  20° C MPa (psi x 103) ASTM-F417 296 (43) 338 (49) 352 (51) 358 (52) 375 (54) 379 (55)
Elastic Modulus  20° C GPa (psi x 106) ASTM-C848 221 (32) 276 (40) 303 (44) 303 (44) 350 (51)  370 (54)
Poisson's Ratio  20° C ASTM-C848 0.22 0.22 0.21 0.21 0.22 0.22
Compressive Strength  20° C MPa (psi x 103) ASTM-C773 1930 (280) 2482 (360) 2103 (305) 2068 (300) 2500 (363) 2600 (377)
Hardness   GPa (kg/mm2) KNOOP 1000 gm 9.4 (960) 10.4 (1058) 11.5 (1175) 11.5 (1175) 13.7 (1400) 14.1 (1440)
    R45N ROCKWELL 45 N     73 75 78 78 82 83
Tensile Strength  25° C MPa (psi x 103) ACMA TEST #4 155 (22) 221 (32) 193 (28) 221 (32) 248 (36) 262 (38)
Fracture Toughness K(I c) Mpa m1/2 NOTCHED BEAM 3 - 4 3 - 4 4 - 5 4 - 5 4 - 5 4 - 5
Thermal Conductivity  20° C W/m °K ASTM-C408 16.0 16.7 22.4 24.7 27.5 30.0
Coefficient of Thermal Expansion 25-1000° C  1X 10-6/°C ASTM-C372 7.2 8.1 8.2 8.2 8.2 8.2
Specific Heat  100° C J/kg*K ASTM-E1269 920 920 880 880 880 880
Thermal Shock Resistance  Δ Tc °C NOTE 3 300 250 250 250 200 200
Maximum Use Temperature   °C NO-LOAD COND. 1400 1500 1700 1700 1700 1750
Impingement   NOTE 4 1.00 0.45 0.52 0.50 0.48 0.47
Rubbing   NOTE 4 1.00 0.36 0.60


Related Links:
Scientific Labware
CoorsTek has provided porcelain and ceramic labware for the scientific community for decades
Plastic Bearings & Bushings
Advanced polymers for high-wear bearings and bushings
Precision Machining and Machine-to-Print Services, Ceramic and Plastic
Seal Components
Spring-Energized Seals, Plastic
Tape and Film, Plastic
Tubes & Rods, Ceramic
Tubes & Rods, Plastic

technical ceramics manufacturing > safety > ceramics for laser equipment components > mining and minerals > food and beverage

 

Terms and Conditions for
Customers and Suppliers

© 2011 CoorsTek, Inc.
legal conditions

[Semiconductor] [Thermal] [Mechanical] [Wear] [Fluid] [Electronic]
   [About CoorsTek] [Contacts] [Products] [Resources and Literature] [Suppliers] [Careers]
      [Deutsch] [Espanol] [Francais] [Italiano] [Korean] [Chinese] [Japanese]