Liquid Phase Sintered Silicon Carbide
Composition
SiC
liquid phase sintered silicon carbide overview
The low porosity microstructure gives liquid phase (LP) sintered silicon carbide its excellent mechanical properties — especially hardness. This makes LP silicon carbide an outstanding material for many different machinery applications.
Example Applications
- Mechanical seals components
- Machinery components
CoorsTek Formulations
Contact a CoorsTek expert to discuss custom solution manufactured from CVD Silicon Carbide to fit your application.
Property | Units | Value |
---|---|---|
Flexural Strength, MOR (20 °C) |
MPa |
600 |
Fracture Toughness, KIc |
MPa m1/2 |
6.3 |
Thermal Conductivity (20 °C) |
W/m K |
80 |
Coefficient of Thermal Expansion |
1 x 10-6/°C |
4.7 |
Maximum Use Temperature |
°C |
- |
Dielectric Strength (6.35mm) |
ac-kV/mm |
- |
Dielectric Loss (tan δ) |
1MHz, 25 °C |
- |
Volume Resistivity (25°C) |
Ω-cm |
0.1 to 105 |
The information provided on this chart is for general material property reference only. The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.