Titanate

Titanate Overview

CoorsTek Titanate formulations are used as dielectric resonators in antennas. The unique dielectric properties of this ceramic allow for improving compactness and efficiency.

CoorsTek Formulations

Contact a CoorsTek expert to discuss a custom manufactured Titanate solution for your application.

Technical Ceramic Chemical Properties iconTechnical Ceramic Electrical Properties iconTechnical Ceramic Mechanical Properties iconTechnical Ceramic Thermal Properties icon

Properties Units Value
Flexural Strength, MOR (20 °C) MPa 105 - 175
Fracture Toughness, KIc MPa m1/2 —

Thermal Conductivity (20 °C)

W/m K 2.1 - 4.2
Coefficient of Thermal Expansion 1x10-6/°C 6.5 - 8.6
Maximum Use Temperature °C —
Dielectric Strength (6.35mm) ac-kV/mm —
Dielectric Loss (tan δ) 1MHz, 25 °C

2.5x10-5 to 3x10-3

Volume Resistivity (25°C) Ω-cm

1010 to 1012