Vehicle Armor

Ground Vehicle Ceramic Armor Components

Vehicle armor modular array manufactured with technical ceramics.

CoorsTek supplies custom ceramic armor components for use in vehicle protection systems. Our lightweight materials help to increase efficiency while meeting or exceeding the performance of traditional steel-based systems.

Advanced Ceramic Vehicle Tiles

Exceptionally well-suited for vehicular applications, CoorsTek produces lightweight technical ceramic tiles using tight-tolerance standards, high-purity formulations, and controlled microstructures to ensure a consistently reliable defense to unexpected threats.

CeraShield™ CERAMIC ARMOR GROUND VEHICLE COMPONENTS

CoorsTek supplies custom ceramic armor components for use in vehicle protection systems. Our lightweight materials help to increase efficiency while meeting or exceeding the performance of traditional steel-based systems.

CoorsTek provides armor components to armor integrators building:

  • Military Vehicles
  • Armored Vehicles
  • Police & SWAT
  • Personal & VIP vehicles
  • Performance Advantages

CoorsTek CeraShield™ ceramics offer many advantages over conventional materials. Our specially formulated ceramic armor materials provide:

  • Low weight
  • High hardness
  • Controlled, uniform microstructures
  • Compatibility for use in finished armor systems with proven performance for national and international ballistic standards

Superior Lightweight Protection Using Next-Generation Ceramic Materials

CoorsTek offers lightweight, superior-quality vehicle armor panels in a wide variety of shapes, sizes, thicknesses, and materials including:

  • CeraShield™ High-Density Aluminum Oxides
    • Traditional monolithic tile material
  • CeraShield Silicon Carbides
    • Superior hardness for advanced threats
    • Lower weight with higher performance benefits
  • CeraShield Boron Carbides
    • Exceedingly hard for extreme energy dissipation
    • Lowest density for ultra-lightweight designs
       

CoorsTek has the capacity to produce vehicle panels at extremely high-volume production while maintaining excellent quality standards through utilizing multiple secure facilities.

Family of various sizes and shapes of silicon carbide vehicle defense armor tiles.

Shapes and Sizes for All Needs

CoorsTek offers CeraShield™ advanced ceramic tiles in a variety of shapes and sizes. Choose from square or hexagon shapes at various imperial and metric measurements, or let our specialists help you select custom shapes, thicknesses, and configurations to optimize your armor system design.

Alumina modular assembly for ballistic vehicle door armor.

Modular Assembly

CoorsTek provides assembly services to form multiple tiles into custom panels of complex shapes and configurations – including holes & cutouts. Perfect for ground vehicles, our modular panels provide a light weight solution, custom fit, and superior performance.

Alumina ballistic vehicle door armor with vacuum-bonding capabilities.

Vacuum-Bonding Capabilities

CoorsTek has perfected the bonding process to perform under some of the harshest industrial environments on the planet. Our specialized process bonds the ceramic to a variety of customer specified substrate materials for a thoroughly robust and integrated solution.