MODEL 101 CERAMIC IGNITER
Time to Temperature
1800F / 982C @ 80volts in 60 seconds
Room Temperature Resistance
40 - 400 ohms
Maximum Temperature
3100°F / 1704°C @ 132 volts
Steady State Current
5.0 amps maximum @ 132 volts
Element Material
Recrystallized silicon carbide
Holder Material
Standard and custom designs available in steatite, cordierite and alumina
Lead Wires and Terminals
Up to 36” in length; rated for 200°C, 250°C, 450°C, or 550°C; various standard terminations available
Control System
Compatible with all leading manufacturer’s systems; no special controls needed to protect igniter
Agency Approval
CSA approved
MODEL 201 CERAMIC IGNITER
Time to Temperature
34 second (typical)
Room Temperature Resistance
40 - 400 ohms
Minimum Temperature
1800°F / 980°C @ 102 volts
Maximum Temperature
3100°F / 1704°C @ 132 volts
Steady State Current
3.5 - 5.0 amps maximum @ 132 volts
Element Material
Recrystallized silicon carbide
Holder Material
Standard and custom designs available in steatite, cordierite, and alumina
Lead Wires and Terminals
Up to 36” in length; rated for 200°C, 250°C, 450°C, or 550°C; various standard terminations available
Control System
Compatible with all leading manufacturer’s systems; no special controls needed to protect igniter
Agency Approval
CSA approved

MODEL 271 CERAMIC IGNITER
Time to Temperature
17 second (typical)
Room Temperature Resistance
40 - 100 ohms
Minimum Temperature
1800°F / 980°C @ 102 volts
Maximum Temperature
3100°F / 1704°C @ 132 volts
Steady State Current
3.5 - 5.0 amps maximum @ 132 volts
Element Material
Recrystallized silicon carbide
Holder Material
Standard and custom designs available in steatite, cordierite, and alumina
Lead Wires and Terminals
Up to 36” in length; rated for 200°C, 250°C, 450°C, or 550°C; various standard terminations available
Control System
Compatible with all leading manufacturer’s systems; no special controls needed to protect igniter
Agency Approval
CSA approved

MODEL 301 CERAMIC IGNITER
Nominal Voltage Rating
12 volts
Time to 1800°F / 980°C
≤ 3 seconds @ 12.0 volts
Minimum Temperature
1895°F / 1035°C @ 10.2 volts
Maximum Temperature
2875°F / 1580°C @ 13.2 volts
Temperature Range @ Nominal Voltage
2102 - 2650°F / 1150-1455°C
Steady-State Current Range
@ Nominal Voltage
@ Nominal Voltage
1.30 - 2.40 amps
Room Temperature Resistance
0.5 - 5 ohms
Element Material
Proprietary ceramic composite
Holder Material
Standard and custom designs in steatite, cordierite, or alumina
Lead Wires
Rated for 200°C, 250°C, 450°C, or 550°C
Terminals
Standard terminals available

MODEL 401 CERAMIC IGNITER
Nominal Voltage Rating
24 volts
Time to 1800°F / 980°C
≤ 3 seconds @ 24.0 volts
Minimum Temperature
1895°F / 1035°C @ 20.4 volts
Maximum Temperature
2875°F / 1580°C @ 26.4 volts
Temperature Range @ Nominal Voltage
2102 - 2650°F / 1150-1455°C
Steady-State Current Range
@ Nominal Voltage
@ Nominal Voltage
1.10 - 2.20 amps
Room Temperature Resistance
1 - 6 ohms
Element Material
Proprietary ceramic composite
Holder Material
Standard and custom designs in steatite, cordierite, or alumina
Lead Wires
Rated for 200°C, 250°C, 450°C, or 550°C
Terminals
Standard terminals available
MODEL 501 CERAMIC IGNITER
Time to Temperature
2000°F / 1100°C within 40 seconds @ 116 volts (typical)
Room Temperature Resistance
40 - 400 ohms
Minimum Temperature
1825°F / 1000°C @ 2.4 amps
Maximum Temperature
2650°F / 1454°C @ 116 volts
Steady State Current
3.2 - 3.6 amps maximum @ 116 volts
Element Material
Recrystallized silicon carbide
Holder Material
Standard and custom designs available in steatite, cordierite, and alumina
Lead Wires and Terminals
Up to 36” in length; rated for 200°C, 250°C, 450°C, or 550°C; various standard terminations available
Control System
Compatible with all leading manufacturer’s systems; no special controls needed to protect igniter
Agency Approval
CSA approved

MODEL 601 CERAMIC IGNITER
Nominal Voltage Rating
120 volts
Time to 1800°F / 980°C
≤ 5 seconds @ 120 volts
Minimum Temperature
1800°F / 980°C @ 102 volts
Maximum Temperature
2875°F / 1580°C @ 132 volts
Temperature Range @ Nominal Voltage
2102 - 2650°F / 1150-1455°C
Steady-State Current Range
@ Nominal Voltage
@ Nominal Voltage
0.40 - 1.20 amps
Room Temperature Resistance
25 - 300 ohms
Element Material
Proprietary ceramic composite
Holder Material
Standard and custom designs in steatite, cordierite, or alumina
Lead Wires
Rated for 200°C, 250°C, 450°C, or 550°C
Terminals
Standard terminals available

MODEL 726 CERAMIC IGNITER
Nominal Voltage Rating
220 volts
Time to 1800°F / 980°C
≤ 7 seconds @ 220 volts
Minimum Temperature
1800°F / 980°C @ 187 volts
Maximum Temperature
2642°F / 1450°C @ 242 volts
Temperature Range @ Nominal Voltage
2102 - 2462°F / 1150-1350°C
Steady-State Current Range
@ Nominal Voltage
@ Nominal Voltage
0.20 - 0.60 amps
Room Temperature Resistance
300 - 2000 ohms
Element Material
Proprietary ceramic composite
Holder Material
Standard and custom designs in steatite, cordierite, or alumina
Lead Wires
Rated for 200°C, 250°C, 450°C, or 550°C
Terminals
Standard terminals available

MODEL 736 CERAMIC IGNITER
Nominal Voltage Rating
230 volts
Time to 1800°F / 980°C
≤ 7 seconds @ 230 volts
Minimum Temperature
1800°F / 980°C @ 195.5 volts
Maximum Temperature
2642°F / 1450°C @ 253 volts
Temperature Range @ Nominal Voltage
2102 - 2462°F / 1150-1350°C
Steady-State Current Range
@ Nominal Voltage
@ Nominal Voltage
0.20 - 0.60 amps
Room Temperature Resistance
300 - 2000 ohms
Element Material
Proprietary ceramic composite
Holder Material
Standard and custom designs in steatite, cordierite, or alumina
Lead Wires
Rated for 200°C, 250°C, 450°C, or 550°C
Terminals
Standard terminals available

MODEL 746 CERAMIC IGNITER
Nominal Voltage Rating
240 volts
Time to 1800°F / 980°C
≤ 7 seconds @ 240 volts
Minimum Temperature
1800°F / 980°C @ 204 volts
Maximum Temperature
2642°F / 1450°C @ 264 volts
Temperature Range @ Nominal Voltage
2102 - 2462°F / 1150-1350°C
Steady-State Current Range
@ Nominal Voltage
@ Nominal Voltage
0.20 - 0.60 amps
Room Temperature Resistance
300 - 2000 ohms
Element Material
Proprietary ceramic composite
Holder Material
Standard and custom designs in steatite, cordierite, or alumina
Lead Wires
Rated for 200°C, 250°C, 450°C, or 550°C
Terminals
Standard terminals available

MODEL 901 DURAGLO CERAMIC IGNITER
Nominal Voltage Rating
120 volts
Time to 1800°F / 980°C
8 Seconds Max @102 Volts
Maximum Temperature
2700°F / 1480°C
Temperature Range @ Nominal Voltage
2202 - 2550°F / 1150-1400°C
Steady-State Current Range
@ Nominal Voltage
@ Nominal Voltage
0.40 - 1.20 amps
Room Temperature Resistance
20 - 100 ohms
Element Material
Proprietary Silicon Nitride
Holder Material
steatite, cordierite, or alumina
Lead Wires
Rated for 200°C, 250°C, 450°C, or 550°C
Terminals
Standard terminals available
CONNECT WITH COORSTEK
- +1 303 271 7100
- +1 855 929 7100 (toll free in North America)
- info@coorstek.com
- Contact CoorsTek Asia
- Contact CoorsTek Europe
- Facility Locations