Ceramic Substrates for Thin-Film Electronics

Alumina Thin Film Substrate Group

CoorsTek is the leader in custom and standard thin-film ceramic substrates. Four thin-film substrate material options combine smooth surface finish, strong flexural strength, and consistent electrical properties. Contact CoorsTek to help you design a specific thin-film substrate for your application, or download our Design Guide.

Why Ceramic Thin-Film Substrates?

Alumina is an optimal material for most thin-film ceramic substrate applications. CoorsTek controls surface finish, grain size, and surface imperfections to enhance fine-line resolution, spacing, and yields in your thin-film process. CoorsTek substrates are available in "as-fired" and finished form, and in both standard and resistor grades. 

When you are facing challenging thermal management issues, aluminum nitride (AlN) substrates help wick heat away from LED, power electronics, and other high-power devices — with thermal conductivity 4-6 higher than alumina substrates.

Superstrate Thin Film Substrates

SuperStrate® Thin-Film Substrates

CoorsTek SuperStrate® substrates are the industry standard for high-performance, thin-film substrates — providing an exceptionally smooth surface finish for optimum fine-line definition.

ADS-996 Thin Film Substrates

ADS-996 Thin-Film Substrates

CoorsTek ADS-996 alumina substrates are a workhorse for most thin-film electronics applications.

ADS-995 Thin Film Substrates

ADS-995 Thin-Film Substrates

Our ADS-995 alumina substrates are an economical alternative for less-demanding thin-film applications.

Thin Film AlN Substrates

Aluminum Nitride Thin-Film Substrates

Aluminum nitride (AlN) substrates are ideal for improved thermal management needed in many LED and power electronics applications, with thermal conductivity 4-6 times higher than other substrates. Learn more

Substrate Size & Thickness

Substrate Thicknesses (Alumina)

CoorsTek offers thin-film substrate thicknesses from 0.127 mm (0.005") to 1.524 mm (0.060"). Standard as-fired thickness tolerance is ± 10%.

Substrate Sizes (Alumina)

CoorsTek offers a wide range of standard and custom sizes. Common square and disc sizes are shown below. Contact us if you need a custom size or geometry.

Thin Film Substrate Size Chart

Lapping & Polishing

All CoorsTek thin-film substrates are available in lapped and polished configurations. In their "as-fired" condition, one side is smoother than the other.

Typical Surface Finish :: Centerline Average (CLA)

Substrate Material

Smooth Side
(as-fired)
Rough Side
(as-fired)
Lapped

Polished

SuperStrate 50 nm 76 nm < 250 nm < 25 nm
ADS-996 76 nm 101 nm < 300 nm < 25 nm
ADS-995 127 nm 178 nm < 762 nm < 50 nm

Laser Machining

Laser Machining for Thin Film Substrates

CoorsTek provides laser machining services for precise hole location,edge definition, and custom shapes and sizes. We also provide design consultation, rapid prototyping, and expedited delivery to get you just what you need, when you need it.

Laser Scribing & Annealing

Side View - Laser Scribed Substrate

CoorsTek offers custom scribing for optimized singulation - defining variable laser pulse spacing and depth in the (x) and (y) scribe directions to control the singulation sequence more precisely. Our enhanced laser scribing helps improve your process yields - preventing hooking, chipping, and premature breakage.

Customer-defined annealing treatments are also available to achieve your specific circuit manufacturing requirements. 

The Thin-Film Substrate Design Guide helps you configure a design from material through finishing and inspection. 

CONNECT WITH COORSTEK




May CoorsTek send you information about our products, services, special offers, news, and events? We will treat your personal data with respect, in accordance with all laws and our Privacy Policy .

Compare 0 materials

You can compare up to 5 materials