Tungsten Carbide (family)
Zirconia (family)
Property | Units | Aluminum Nitride (family) | Silicon Carbide (family) | Specialty (family) | Composites (family) | Alumina (family) | Boron Carbide (family) | Silicates (family) | Silicon Nitride (family) | Tungsten Carbide (family) | Zirconia (family) |
---|---|---|---|---|---|---|---|---|---|---|---|
Coefficient of Thermal Expansion |
1 x 10-6/°C |
3.3 - 5.6 |
3.0 - 4.8 |
7.2 - 9.1 |
4.5 - 4.9 |
3.5 - 10 |
2.9 - 4.5 |
5.1 - 5.9 |
10 - 11 |
||
Dielectric Loss (tan δ) |
1MHz, 25 °C |
10-4 to 7.7 x 10-3 |
- |
10-4 to 0.02 |
- |
0.002 - 7 |
10-4 to 1.2 x 10-3 |
- |
10-3 |
||
Dielectric Strength (6.35mm) |
ac-kV/mm |
15 - 25 |
- |
5.3 - 19.7 |
- |
9.8 - 10 |
15.0 -17.7 |
- |
9.0 - 9.4 |
||
Flexural Strength, MOR (20 °C) |
MPa |
260 - 460 |
210 - 700 |
250 - 1250 |
250 - 450 |
20 - 170 |
600 - 1000 |
900 - 2330 |
180 - 1720 |
||
Fracture Toughness, KIc |
MPa m1/2 |
2.75 - 6.0 |
3.5 - 6.3 |
3.0 - 7.3 |
3.0 - 5.0 |
2.0 |
4.25 - 7.5 |
1.0 - 7.0 |
3.5 - 13.0 |
||
Maximum Use Temperature |
°C |
800 |
1000 - 1600 |
1200 - 1800 |
1000 - 2000 |
1200 - 1700 |
1150 - 1400 |
103 |
500 - 2400 |
||
Thermal Conductivity (20 °C) |
W/m K |
80 - 205 |
80 - 225 |
12.0 - 37.1 |
43 - 100 |
2.5 - 7.3 |
19 -100 |
1.4 - 100 |
2.0 - 2.5 |
||
Volume Resistivity (25°C) |
Ω-cm |
1011 to > 1014 |
0.1 - 105 |
1014 to > 1015 |
103 |
1010 to > 1014 |
1010 to 1014 |
103 |
108 to 1.3 x 1014 |
||