Mullite

Composition

Al Silicate

mullite overview

Mullite has excellent thermal shock resistance and dielectric strength, making it ideal for electronic components for manufacturing purposes.

Example Applications

  • Ceramic tubes
  • Metal foundry filters

CoorsTek Formulations

Contact a CoorsTek expert to choose a mullite solution for your application.

Property Units Value

Flexural Strength, MOR (20 °C)

MPa

45 - 170

Fracture Toughness, KIc

MPa m1/2

2.0

Thermal Conductivity (20 °C)

W/m K

4.0

Coefficient of Thermal Expansion

1 x 10-6/°C

4.0 - 5.0

Maximum Use Temperature

°C

1700

Dielectric Strength (6.35mm)

ac-kV/mm

9.8 - 10.0

Dielectric Loss (tan δ)

1MHz, 25 °C

0.002

Volume Resistivity (25°C)

Ω-cm

1010 to 1014

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.