Steatite
Composition
Mg Silicate
steatite overview
Steatite is used in electronic components and manufacturing processes. Its low dielectric loss combined with a high dielectric strength make it an excellent inexpensive component for electronics and manufacturing processes.
Example Applications
- Traditional electrical insulators
- Fuses
CoorsTek Expertise
Contact a CoorsTek expert to choose a steatite solution for your application.
Property | Units | Value |
---|---|---|
Flexural Strength, MOR (20 °C) |
MPa |
140 - 160 |
Fracture Toughness, KIc |
MPa m1/2 |
2.0 |
Thermal Conductivity (20 °C) |
W/m K |
2.5 - 3.0 |
Coefficient of Thermal Expansion |
1 x 10-6/°C |
8.5 - 10.0 |
Maximum Use Temperature |
°C |
1200 |
Dielectric Strength (6.35mm) |
ac-kV/mm |
- |
Dielectric Loss (tan δ) |
1MHz, 25 °C |
- |
Volume Resistivity (25°C) |
Ω-cm |
1013 |
The information provided on this chart is for general material property reference only. The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.
CONNECT WITH COORSTEK
- +1 303 271 7100
-
+1 855 929 7100
(toll free in North America)
-
Email
info@coorstek.com - Contact Corporate Headquarters
- Contact CoorsTek Asia
- Contact CoorsTek Europe
- Facility Locations