Carbon / Graphite
Composition
C
carbon / graphite overview
CoorsTek carbon and graphite both have high purity, thermal conductivity, and electrical conductance. The unique combination of purity and thermal conductivity prevents contamination and thermal shock: making the material ideal for both semiconductor manufacturing and high-strength electronics.
Different coatings can be applied to augment the material properties. Additionally, the low electrical resistivity and high thermal conductivity makes carbons ideal for maintaining a lower operating temperature in heat generating electrical parts like motor brushes.
- Electrical conductance
- High purity
- Thermal shock resistance
- Thermal conductivity
Example Applications
- Motor brushes
- Crucibles
CoorsTek Formulations
Contact a CoorsTek expert to choose a Carbon solution for your application.
Property | Units | Value |
---|---|---|
Flexural Strength, MOR (20 °C) |
MPa |
40 - 300 |
Fracture Toughness, KIc |
MPa m1/2 |
- |
Thermal Conductivity (20 °C) |
W/m K |
107 - 340 |
Coefficient of Thermal Expansion |
1 x 10-6/°C |
- |
Maximum Use Temperature |
°C |
1500 - 3000 |
Dielectric Strength (6.35mm) |
ac-kV/mm |
- |
Dielectric Loss (tan δ) |
1MHz, 25 °C |
- |
Volume Resistivity (25°C) |
Ω-cm |
- |
The information provided on this chart is for general material property reference only. The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.