Composition

TiB2

titanium diboride overview

Titanium Diboride (TiB2) is an extremely hard ceramic used, for example, in specialized ballistic armor applications. Additionally, unlike most ceramic compositions, it is electrically conductive.

Example Applications

  • Ballistic armor components

 

CoorsTek Formulations

Contact a CoorsTek expert to discuss a custom manufactured Titanium Diboride solution for your application.

Property Units Value

Flexural Strength, MOR (20 °C)

MPa

275

Fracture Toughness, KIc

MPa m1/2

6.9

Thermal Conductivity (20 °C)

W/m K

-

Coefficient of Thermal Expansion

1 x 10-6/°C

8.0

Maximum Use Temperature

°C

-

Dielectric Strength (6.35mm)

ac-kV/mm

-

Dielectric Loss (tan δ)

1MHz, 25 °C

-

Volume Resistivity (25°C)

Ω-cm

-

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.

CONNECT WITH COORSTEK




May CoorsTek send you information about our products, services, special offers, news, and events? We will treat your personal data with respect, in accordance with all laws and our Privacy Policy .

Compare 0 materials

You can compare up to 5 materials