CoorsTek

Home

+1 303 271 7100

Contact

Fully Stabilized Zirconia

Composition

Fully Stabilized ZrO2

fully stabilized zirconia overview

Fully Stabilized Zirconia is applied in high-temperature applications that require strong thermal shock resistance, fracture toughness, and superior corrosion resistance. Additionally, Fully Stabilized Zirconia has the unique capability to allow oxygen ion transporting, meaning only oxygen ions can pass through its structure. This allows it to be used in applications like active membranes.

Example Applications

  • O2 detection sensor components
  • Thermal shock crucibles

 

CoorsTek Formulations

Contact a CoorsTek expert to discuss custom manufactured Fully Stabilized Zirconia solution for your application.

Property Units Value

Flexural Strength, MOR (20 °C)

MPa

180-193

Fracture Toughness, KIc

MPa m1/2

4.0

Thermal Conductivity (20 °C)

W/m K

2.5

Coefficient of Thermal Expansion

1 x 10-6/°C

10.5-11.0

Maximum Use Temperature

°C

1800-2400

Dielectric Strength (6.35mm)

ac-kV/mm

-

Dielectric Loss (tan δ)

1MHz, 25 °C

-

Volume Resistivity (25°C)

Ω-cm

108-1014

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.