CoorsTek Introduces High-Performance Aluminum Nitride Substrates

February 12 2013

Likely the largest provider of ceramic substrates for decades, CoorsTek expands product line to include high heat dissipation aluminum nitride substrates.

February 12, 2013 – Golden, Colorado – CoorsTek, the world’s largest technical ceramics manufacturer, today announced introduction of aluminum nitride substrates. Ideal for the rapidly growing LED market and other markets where high heat dissipation is useful, these ceramic substrates boast a thermal conductivity of 170 W/m K. 

CoorsTek AlN (aluminum nitride) ceramic substrates feature a very high dielectric strength, are a non-toxic alternative to BeO (beryllium oxide), and exhibit a thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors.

“While we already offer an extensive line of ceramic substrates, our new high performance aluminum nitride substrates cover high heat dissipation applications,” says Andrew Golike, Electronics General Manager for CoorsTek, Inc. “We’ve ramped our production and finishing services to ensure an on-time delivery for our customers,” he continues.

Brochure link

http://www.coorstek.com/resource-library/library/8510-1843- Aluminum_Nitride_Substrates.pdf

More about CoorsTek

Established in 1910, CoorsTek is the largest technical ceramics manufacturer in the world with over 40 facilities in the Americas, Europe, and Asia. CoorsTek supplies critical components and complete assemblies for defense, medical, automotive, semiconductor, aerospace, electronic, power generation, telecommunication, and other high-technology markets. Utilizing advanced material technologies, the company’s engineered solutions enable its customers’ products to overcome technological barriers and improve performance. For more information, please visit www.coorstek.com.

CONNECT WITH COORSTEK




May CoorsTek send you information about our products, services, special offers, news, and events? We will treat your personal data with respect, in accordance with all laws and our Privacy Policy .

Compare 0 materials

You can compare up to 5 materials