CoorsTek

Home

+1 303 271 7100

Contact

Titanate

Composition

TiO2

titanate overview

CoorsTek Titanate formulations are used as dielectric resonators in antennas. The unique dielectric properties of this ceramic allow for improving compactness and efficiency.

Example Applications

  • Antennas
  • Resonators

 

CoorsTek Formulations

Contact a CoorsTek expert to choose a Titanate solution for your application.

Property Units Value

Flexural Strength, MOR (20 °C)

MPa

105 - 175

Fracture Toughness, KIc

MPa m1/2

-

Thermal Conductivity (20 °C)

W/m K

2.1 - 4.2

Coefficient of Thermal Expansion

1 x 10-6/°C

6.5 - 8.6

Maximum Use Temperature

°C

-

Dielectric Strength (6.35mm)

ac-kV/mm

-

Dielectric Loss (tan δ)

1MHz, 25 °C

2.5 x 10-5 to 3 x 10-3

Volume Resistivity (25°C)

Ω-cm

1010 to 1012

The information provided on this chart is for general material property reference only.  The customer should recognize that exact properties of materials may vary according to product configuration but close control of values of most properties can be maintained, if specified. Nothing herein is provided, or is to be construed, as absolute engineering data or constituting a warranty or representation. Contact CoorsTek for cost-effective design, development and manufacturing assistance. CoorsTek has 300+ variations including various forming and firing processes, not all variants are represented in the present website.

CONNECT WITH COORSTEK

Ask A Question

Thank you for contacting us.

Compare 0 materials

You can compare up to 5 materials